Physical and Mechanical Properties

The chemical composition of alloys and have been optimized in collaboration with our customers in order to maximize the behavior of the metal under the most stringent conditions of seawater corrosion.
Additionally, and meet all requirements of most international standards.

Physical Properties

Typical values Units
Density (20°C) kg/m3 8900 8900
Electrical resistivity (20°C annealed) μΩ.cm 19 34
Thermal conductivity (20° to 200°C) W/m.°K 50 30
Coefficient of expansion (20° to 200°C) C x 10-6 17 16
Modulus of elasticity (20°C annealed) MPa 126 000 126 000
Annealing temperature °C 760-800 780-820
Melting interval °C 1100-1150 1180-1240
Magnetic Permeability (20° annealed)   1.08 - 1.80 <1.05

Mechanical Properties (Annealed Temper)

Typical values Units
Tensile strength (UTS), (Rm) MPa ≥ 310 ≥ 350
  ksi ≥ 44 ≥ 51
Proof stress (YS 0,2), (Rp 0,2) MPa ≥ 110 ≥ 130
  ksi ≥ 16 ≥ 19
Elongation ( E 5,65 √S) % ≥ 35 ≥ 30
Hardness (HB10 D²)   ≥ 70 ≥ 80

Mechanical Properties According to Temperature

°C   -200 -150 -100 -50 0 50 100 150 200 250 300 350
  Unit                        
                         
T.S MPa 450 390 330 310 300 300 290 280 270 260 250 230
Y.S. MPa 150 145 140 130 100 100 100 95 90 85 80 65
E ( E 5,65 S) % >         35 32 28 26 24 23 21 20
                         
T.S MPa 480 420 380 360 350 350 340 320 320 310 300 280
Y.S. MPa 110 175 150 140 130 130 130 125 120 115 110 100
E ( E 5,65 S) % >         30 28 24 23 22 20 19 18

Contrary to steel, and does not become brittle at low temperatures